Subject: Blending PP with PE
From: nick
Newsgroups: sci.polymers
Followup: sci.polymers
Organization: Newsgroupdirect
Date: Wed, 25 Jul 2018 00:18 UTC
Path: eternal-september.org!news.eternal-september.org!reader01.eternal-september.org!reader01.eternal-september.org!reader02.eternal-september.org!feeder.eternal-september.org!border1.nntp.ams1.giganews.com!nntp.giganews.com!feeds.phibee-telecom.net!newsfeed.xs4all.nl!newsfeed7.news.xs4all.nl!85.12.16.68.MISMATCH!peer01.ams1!peer.ams1.xlned.com!news.xlned.com!peer03.am4!peer.am4.highwinds-media.com!news.highwinds-media.com!fx09.am4.POSTED!not-for-mail
Subject: Blending PP with PE
From: 0f8503901d844703eea1acecb7a4938a_2301@example.com (nick)
Sender: nick <0f8503901d844703eea1acecb7a4938a_2301@example.com>
Newsgroups: sci.polymers
Followup-To: sci.polymers
Content-Type: text/plain; charset="iso-8859-1"; format="flowed"
Content-Transfer-Encoding: 8bit
User-Agent: Hermes v1.4
Injection-Info: fcc304c7dbe9e9423a7b6bf47b4c9fce;0236c97cb77f1ded18411a52c654a3ef
Lines: 8
Message-ID: <_kP5D.2107606$sc1.742886@fx09.am4>
X-Complaints-To: abuse@newsgroupdirect.com
NNTP-Posting-Date: Wed, 25 Jul 2018 00:18:02 UTC
Organization: Newsgroupdirect
Date: Wed, 25 Jul 2018 00:18:02 GMT
X-Received-Bytes: 952
X-Received-Body-CRC: 627430777
View all headers

Hi.
I want to blend PP with PE to format a mix that can be extruded. Since these
are not miscible, what can I add as a modifier to make them miscible

--
for full context, visit https://www.polytechforum.com/polymers/blending-pp-with-pe-10036-.htm

Subject: Blending PP with PE
From: htnmate@yahoo.com
Newsgroups: sci.polymers
Date: Sun, 9 Sep 2018 15:51 UTC
References: 1
X-Received: by 2002:a0c:d01c:: with SMTP id u28-v6mr5727011qvg.30.1536508263465;
Sun, 09 Sep 2018 08:51:03 -0700 (PDT)
X-Received: by 2002:a81:2b43:: with SMTP id r64-v6mr170749ywr.1.1536508263226;
Sun, 09 Sep 2018 08:51:03 -0700 (PDT)
Path: eternal-september.org!news.eternal-september.org!reader01.eternal-september.org!reader01.eternal-september.org!reader02.eternal-september.org!feeder.eternal-september.org!weretis.net!feeder4.news.weretis.net!newsreader4.netcologne.de!news.netcologne.de!peer03.ams1!peer.ams1.xlned.com!news.xlned.com!peer03.fr7!futter-mich.highwinds-media.com!peer02.iad!feed-me.highwinds-media.com!news.highwinds-media.com!z10-v6no1559891qtb.0!news-out.google.com!k67-v6ni844qte.1!nntp.google.com!z10-v6no1559884qtb.0!postnews.google.com!glegroupsg2000goo.googlegroups.com!not-for-mail
Newsgroups: sci.polymers
Date: Sun, 9 Sep 2018 08:51:02 -0700 (PDT)
In-Reply-To: <_kP5D.2107606$sc1.742886@fx09.am4>
Complaints-To: groups-abuse@google.com
Injection-Info: glegroupsg2000goo.googlegroups.com; posting-host=185.216.35.251;
posting-account=AkF9BgoAAAC8kCdMe5MDduI9lijpEqwx
NNTP-Posting-Host: 185.216.35.251
References: <_kP5D.2107606$sc1.742886@fx09.am4>
User-Agent: G2/1.0
MIME-Version: 1.0
Message-ID: <14c3a36a-23a2-47e1-bd61-f109aadab520@googlegroups.com>
Subject: Blending PP with PE
From: htnmate@yahoo.com
Injection-Date: Sun, 09 Sep 2018 15:51:03 +0000
Content-Type: text/plain; charset="UTF-8"
X-Received-Bytes: 1327
X-Received-Body-CRC: 203566698
View all headers

Try Fusabond:

http://www.dupont.com/products-and-services/additives-modifiers/polymer-additives/articles/polymer-compatibilizer-for-recycling.html