Rocksolid Light

News from da outaworlds

mail  files  register  groups  login

Message-ID:  

You recoil from the crude; you tend naturally toward the exquisite.


sci / sci.polymers / Re: Proper way to melt nylon

SubjectAuthor
o Re: Proper way to melt nylonRick Silling

1
Subject: Re: Proper way to melt nylon
From: Rick Silling
Newsgroups: sci.polymers
Date: Sun, 9 Jan 2022 22:29 UTC
References: 1
X-Received: by 2002:ad4:5e88:: with SMTP id jl8mr27902037qvb.90.1641767394558;
Sun, 09 Jan 2022 14:29:54 -0800 (PST)
X-Received: by 2002:a9d:206a:: with SMTP id n97mr54998283ota.142.1641767394287;
Sun, 09 Jan 2022 14:29:54 -0800 (PST)
Path: eternal-september.org!news.eternal-september.org!reader01.eternal-september.org!reader02.eternal-september.org!news.misty.com!border2.nntp.dca1.giganews.com!nntp.giganews.com!news-out.google.com!nntp.google.com!postnews.google.com!google-groups.googlegroups.com!not-for-mail
Newsgroups: sci.polymers
Date: Sun, 9 Jan 2022 14:29:54 -0800 (PST)
In-Reply-To: <1152024753.775492.9930@m73g2000cwd.googlegroups.com>
Injection-Info: google-groups.googlegroups.com; posting-host=72.84.102.40; posting-account=aGAjKwoAAADKTMCkOKe-NKvf9Hkw0eWm
NNTP-Posting-Host: 72.84.102.40
References: <1152024753.775492.9930@m73g2000cwd.googlegroups.com>
User-Agent: G2/1.0
MIME-Version: 1.0
Message-ID: <f8a640a3-769b-4610-b65d-0d4bf33032ben@googlegroups.com>
Subject: Re: Proper way to melt nylon
From: rick.silling@gmail.com (Rick Silling)
Injection-Date: Sun, 09 Jan 2022 22:29:54 +0000
Content-Type: text/plain; charset="UTF-8"
Lines: 8
View all headers

On Tuesday, July 4, 2006 at 10:52:33 AM UTC-4, boardjunkie wrote:
> Fishing for information on do's and don'ts when melting nylon. What I
> need to do is liquify a relatively small amount to dip wood drumstick
> tips in to keep them from chipping. I figure weed eater line is a cheap
> source for the nylon. Is this something I'd want to attempt to do over
> a gas stove in a junk pan? I'm not sure if it will bubble and get
> messy......molten nylon is not my idea of snappy attire. So.....any
> advise?
Just melt the damn stuff & be careful not to set it ablaze. Drip it into a form of desired shape & hey people, ever heard of common sense ?