sci / sci.polymers / Re: What solvents dissolve PMMA?

SubjectAuthor
* Re: What solvents dissolve PMMA?mohsinkhalid133
`- Re: What solvents dissolve PMMA?Isha Arora

1
Subject: Re: What solvents dissolve PMMA?
From: mohsinkhalid133@gmail.com
Newsgroups: sci.polymers
Date: Mon, 9 Mar 2020 18:30 UTC
References: 1
X-Received: by 2002:ac8:4792:: with SMTP id k18mr15681988qtq.192.1583778618945;
Mon, 09 Mar 2020 11:30:18 -0700 (PDT)
X-Received: by 2002:a81:1193:: with SMTP id 141mr9577082ywr.165.1583778618640;
Mon, 09 Mar 2020 11:30:18 -0700 (PDT)
Path: eternal-september.org!news.eternal-september.org!reader01.eternal-september.org!reader01.eternal-september.org!feeder.eternal-september.org!news.gegeweb.eu!gegeweb.org!usenet-fr.net!proxad.net!feeder1-2.proxad.net!209.85.160.216.MISMATCH!news-out.google.com!nntp.google.com!postnews.google.com!google-groups.googlegroups.com!not-for-mail
Newsgroups: sci.polymers
Date: Mon, 9 Mar 2020 11:30:18 -0700 (PDT)
In-Reply-To: <a7edb004.0306171253.318e0801@posting.google.com>
Complaints-To: groups-abuse@google.com
Injection-Info: google-groups.googlegroups.com; posting-host=39.36.169.49; posting-account=IaMcJwkAAADiSz32nmkUsUKip9nj8bmA
NNTP-Posting-Host: 39.36.169.49
References: <a7edb004.0306171253.318e0801@posting.google.com>
User-Agent: G2/1.0
MIME-Version: 1.0
Message-ID: <317f134f-49f1-47d6-b314-715b5469f3d6@googlegroups.com>
Subject: Re: What solvents dissolve PMMA?
From: mohsinkhalid133@gmail.com
Injection-Date: Mon, 09 Mar 2020 18:30:18 +0000
Content-Type: text/plain; charset="UTF-8"
View all headers

On Wednesday, 18 June 2003 01:53:08 UTC+5, Mike VM wrote:
> Does anybody know where I could get information as to what common
> solvents (IPA, methanol, acetone, etc.) dissolve (or don't dissolve)
> PMMA?
>
> For a more general question: What is the best resource on the Web for
> finding out what solvents attack a given material?
>
> Thanks,
>
> Mike VM

PMMA easily dissolve in Acetone at room temperature and in DMF too

Subject: Re: What solvents dissolve PMMA?
From: Isha Arora
Newsgroups: sci.polymers
Date: Tue, 1 Dec 2020 13:49 UTC
References: 1 2
X-Received: by 2002:ac8:6b49:: with SMTP id x9mr2828037qts.197.1606830585998; Tue, 01 Dec 2020 05:49:45 -0800 (PST)
X-Received: by 2002:a9d:5549:: with SMTP id h9mr1764601oti.230.1606830585530; Tue, 01 Dec 2020 05:49:45 -0800 (PST)
Path: eternal-september.org!news.eternal-september.org!reader01.eternal-september.org!reader02.eternal-september.org!news.uzoreto.com!tr2.eu1.usenetexpress.com!feeder.usenetexpress.com!tr2.iad1.usenetexpress.com!border1.nntp.dca1.giganews.com!nntp.giganews.com!news-out.google.com!nntp.google.com!postnews.google.com!google-groups.googlegroups.com!not-for-mail
Newsgroups: sci.polymers
Date: Tue, 1 Dec 2020 05:49:45 -0800 (PST)
In-Reply-To: <317f134f-49f1-47d6-b314-715b5469f3d6@googlegroups.com>
Complaints-To: groups-abuse@google.com
Injection-Info: google-groups.googlegroups.com; posting-host=103.27.9.50; posting-account=drI1lgoAAAB1Sqecxr__mIu7tPq1mbpl
NNTP-Posting-Host: 103.27.9.50
References: <a7edb004.0306171253.318e0801@posting.google.com> <317f134f-49f1-47d6-b314-715b5469f3d6@googlegroups.com>
User-Agent: G2/1.0
MIME-Version: 1.0
Message-ID: <4385e964-2fd1-4642-8034-ffbd7f410dden@googlegroups.com>
Subject: Re: What solvents dissolve PMMA?
From: arora.isha1993@gmail.com (Isha Arora)
Injection-Date: Tue, 01 Dec 2020 13:49:45 +0000
Content-Type: text/plain; charset="UTF-8"
Lines: 13
View all headers

On Tuesday, March 10, 2020 at 12:00:20 AM UTC+5:30, mohsink...@gmail.com wrote:
> On Wednesday, 18 June 2003 01:53:08 UTC+5, Mike VM wrote:
> > Does anybody know where I could get information as to what common
> > solvents (IPA, methanol, acetone, etc.) dissolve (or don't dissolve)
> > PMMA?
> >
> > For a more general question: What is the best resource on the Web for
> > finding out what solvents attack a given material?
> >
> > Thanks,
> >
> > Mike VM
> PMMA easily dissolve in Acetone at room temperature and in DMF too
Can anyone please help me in knowing the mixing ratios for PMMA in THF